The crew at V&C Metal Polishing began by sanding off all the pitting and oxidized aluminum from the surface of the grilles and bezels first using a 120-grit sanding belt and progressing to 300-grit paper. Areas too small to reach with the belt are buffed with smaller wheels or a hand-held disc sander. If the pitting isn’t removed, the pores in surface of the aluminum remain open and the pits can reappear after anodizing.
Aluminum Grille Resto

The crew at V&C Metal Polishing began by sanding off all the pitting and oxidized aluminum from the surface of the grilles and bezels first using a 120-grit sanding belt and progressing to 300-grit paper. Areas too small to reach with the belt are buffed with smaller wheels or a hand-held disc sander. If the pitting isn’t removed, the pores in surface of the aluminum remain open and the pits can reappear after anodizing.  View Related Article

 